So, I’m working on a commission, and it’s over 100 degrees in my area of the country.

I took 54 15mm models outside to prime and what a catastrophe.  I’ve primed in various temperatures before, but this time, the models are dusted.  The primer didn’t stick and it’s like dust on the models.

Some cleaning, and they will be fine.  But, just a reminder to prime in ideal conditions.  Things I’ve known, but never quite experienced.  Chalk that one up to relying on chance.